The 15-5 alloy was designed to have greater toughness than 17-4 PH. The 15-5 alloy is martensitic in structure in the annealed condition and is further strengthened by a relatively low temperature heat treatment which precipitates a copper containing phase in the alloy.

International shipping is available on all Sidhant metals. To request a quote, please CLICK HERE.

15/5 Plate

GRADE
THICKNESS 15/5PH Annealed) 15/5PH H925 15/5PH H1025 15/5PH H1075 15/5PH H1100
0.188 x x
0.625 x x x
0.75 x
1.000 x x
1.2500 x x
1.500 x x x